High-temperature Oxidation of Fe-Cr Steels in Steam Condition – A Review
DOI:
https://doi.org/10.17509/ijost.v1i1.2217Keywords:
Steam oxidation, Power plant, Ferritic steel, BoilerAbstract
The development of supercritical (SC) and ultra-supercritical (USC) power plants requires materials with better corrosion properties. Deep understanding on the oxidation mechanism in the boiler environment is one of the important factors to support this development. In this work, high temperature oxidation of Fe-Cr steels in steam condition is reviewed. Several mechanisms that explain the effect of water vapor in the oxidation behavior the steel were presented.
Downloads
References
Ani, M. H., Kodama, T., Ueda, M., Kawamura, K., and Maruyama, T. (2009). The effect of water vapor on high temperature oxidation of Fe-Cr alloys at 1073 K. Materials transactions, 50(11), 2656-2663. DOI: https://doi.org/10.2320/matertrans.M2009212
Asteman, H., Svensson, J. E. and Johansson, L. G. (2002). Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate. Oxidation of metals, 57(3), 193–216. DOI: https://doi.org/10.1023/A:1014877600235
Asteman, H., Svensson, J. E., Norell, M. and L.G. Johansson, L. G. (2000). Influence of water vapor and flow rate on the high-temperature oxidation of 304L; Effect of chromium oxide hydroxide evaporation. Oxidation of metals. 54(1), 11–26. DOI: https://doi.org/10.1023/A:1004642310974
Ennis, P., and Quadakkers, W. (2007). Implications of steam oxidation for the service life of high-strength martensitic steel components in high-temperature plant. International journal of pressure vessels and piping, 84(1-2), 82-87. DOI: https://doi.org/10.1016/j.ijpvp.2006.09.008
Ehlers, J., Young, D., Smaardijk, E., Tyagi, A., Penkalla, H., Singheiser, L., and Quadakkers, W. (2006). Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments. Corrosion science, 48(11), 3428-3454. DOI: https://doi.org/10.1016/j.corsci.2006.02.002
Essuman, E., Meier, G., Żurek, J., Hänsel, M., Singheiser, L., and Quadakkers, W. (2007). Enhanced internal oxidation as trigger for breakaway oxidation of Fe–Cr alloys in gases containing water vapor. Scripta materialia, 57(9), 845-848.
Essuman, E., Meier, G., Żurek, J., Hänsel, M., Singheiser, L., and Quadakkers, W. (2007). Enhanced internal oxidation as trigger for breakaway oxidation of Fe–Cr alloys in gases containing water vapor. Scripta materialia, 57(9), 845-848. DOI: https://doi.org/10.1016/j.scriptamat.2007.06.058
Huang, J., Zhou, K., Xu, J., and Bian, C. (2013). On the failure of steam-side oxide scales in high temperature components of boilers during unsteady thermal processes. Journal of loss prevention in the process industries, 26(1), 22-31. DOI: https://doi.org/10.1016/j.jlp.2012.08.004
Kurniawan, T. (2013a). Hydrogen permeability in the scales of iron oxide at 973 K under constant oxygen activity (Doctoral dissertation, Tokyo Institute of Technology).
Kurniawan, T., Ueda, M., Kawamura, K., and Maruyama, T. (2013b). Phase stability of iron oxides on palladium–iron alloy at elevated temperatures and its application to high temperature oxidation. Materials transactions, 54(9), 1829-1837. DOI: https://doi.org/10.2320/matertrans.M2013122
Lepingle, V., Louis, G., Allué, D., Lefebvre, B., and Vandenberghe, B. (2008). Steam oxidation resistance of new 12%Cr steels: Comparison with some other ferritic steels. Corrosion science, 50(4), 1011-1019. DOI: https://doi.org/10.1016/j.corsci.2007.11.033
McKendry, P. (2002). Energy production from biomass (part 2): conversion technologies. Bioresource technology, 83(1), 47-54. DOI: https://doi.org/10.1016/S0960-8524(01)00119-5
Nakagawa, K., Matsunaga, Y., and Yanagisawa, T. (2001). Corrosion behavior of ferritic steels on the air sides of boiler tubes in a steam/air dual environment. Materials at high temperatures, 18(1), 51-56. DOI: https://doi.org/10.1179/mht.2001.005
Nakagawa, K., Matsunaga, Y., and Yanagisawa, T. (2003). Corrosion behavior of ferritic steels on the air sides of boiler tubes in a steam/air dual environment. Materials at high temperatures, 20(1), 67-73. DOI: https://doi.org/10.1179/mht.2003.010
Nakai, M., Nagai, K., Murata, Y., Morinaga, M., Matsuda, S., and Kanno, M. (2005). Correlation of high-temperature steam oxidation with hydrogen dissolution in pure iron and ternary high-chromium ferritic steel. ISIJ Int. ISIJ international, 45(7), 1066-1072. DOI: https://doi.org/10.2355/isijinternational.45.1066
Setiawan, A. R., Ani, M. H., Ueda, M., Kawamura, K., and Maruyama, T. (2010). Oxygen permeability through internal oxidation zone in Fe–Cr alloys under dry and humid conditions at 973 and 1 073 K. ISIJ Int. ISIJ international, 50(2), 259-263. DOI: https://doi.org/10.2355/isijinternational.50.259
Ueda, M., Maruyama, T. (2005). High temperature steam oxidation of high Cr ferritic steels. Zairyou-to-Kanyou, 54(5), 175-182. DOI: https://doi.org/10.3323/jcorr1991.54.175
Viswanathan, R., Henry, J., Tanzosh, J., Stanko, G., Shingledecker, J., Vitalis, B., and Purgert, R. (2005). U.S. Program on materials technology for ultra-supercritical coal power plants. Journal of materials engineering and performance, 14(3), 281-292. DOI: https://doi.org/10.1361/10599490524039
Żurek, J., Wessel, E., Niewolak, L., Schmitz, F., Kern, T., Singheiser, L., and Quadakkers, W. (2004). Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650 °C. Corrosion science, 46(9), 2301-2317. DOI: https://doi.org/10.1016/j.corsci.2004.01.010
Downloads
Published
Issue
Section
License

This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.